| Item number | CAS number | Number | Packaging | Parameter |
| 100044 | 7782-42-5 | XF057 | 100 g | Expansion ratio: over 350 times, starting temperature 200°C |
| 101389 | 7782-42-5 | XF057 | 500 g | Expansion ratio: over 350 times, starting temperature 200°C |
| 101390 | 7782-42-5 | XF057 | 1 kg | Expansion ratio: over 350 times, starting temperature 200°C |
Product Name
Chinese Name: High-Quality Expandable Graphite
I'd be happy to help translate Chinese to English while preserving HTML tags, numbers, and technical terms. However, I don't see any Chinese text in your message. Could you please provide the Chinese text you'd like me to translate?Expandable Graphite
Nature
Form: Black powder
Parameter
Expansion ratio:350more than double
Preparation process: Raise the furnace temperature to 950-980 degrees Celsius, and place the sample inside for about 20 seconds.
Starting temperature:200Degree
Carbon content: 92-95wt%
Particle size: ~300μm (50 mesh)
Application
NA