Ternary Nickel-Cobalt-Manganese Precursor Mixer
Material Name: Ternary Nickel-Cobalt-Manganese Precursor
Basic characteristics of the material: Bulk density: 1.4-1.6 g/cm³; Laser particle size (D50): 8-12 μm.
Material status: dry powder
Equipment Technical Requirements
Mixing time: ≥40min
Production capacity: 7t/d
Single mixing capacity: 6t
Loading factor: 0.6
Operating Pressure: Normal Pressure
Equipment appearance requirements: polished finish.
Rotate to horizontal mixer
The equipment material should be...
Material: Stainless steel 304. The equipment cylinder, cylinder cover, and internal and external ribbon main shaft are sprayed with Harla (ECTFE) to a thickness of 0.5mm.
Quantity: one unit